Title: MAXIMUM LIKELIHOOD CURVES FOR MULTIPLE OBJECTS EXTRACTION: APPLICATION TO RADIOGRAPHIC INSPECTION FOR WELD DEFECTS DETECTION
Issue Number: | Vol. 1, No. 1 |
Year of Publication: | May - 2011 |
Page Numbers: | 209-222 |
Authors: | Aicha Baya Goumeidane, Mohammed Khamadja, Nafaa Nacereddine |
Journal Name: | International Journal of New Computer Architectures and their Applications (IJNCAA) - Hong Kong |
Abstract:
This paper presents an adaptive probabilistic region-based deformable model using an explicit representation that aims to extract automatically defects from a radiographic film. To deal with the height computation cost of such model, an adaptive polygonal representation is used and the search space for the greedy-based model evolution is reduced. Furthermore, we adapt this explicit model to handle topological changes in presence of multiple defects.